incoloy 625 ngongo ngongo kapi
C | Cr | Ni | Fe | Mn | Si | Mo | Co | P | S | Ti | Nb + Ta | Al |
---|---|---|---|---|---|---|---|---|---|---|---|---|
≤ 0.1 | 20 – 23 | ≥ 58 | ≤ 5 | ≤ 0.5 | ≤ 0.5 | 8 – 10 | ≤ 1* | ≤ 0.015 | ≤ 0.015 | ≤ 0.4 | 3.15 – 4.15 | ≤ 0.4 |
(papatipu%)
* Mena kua whakatauhia
ASTM B444, ASME SB444, AMS 5581
Mo te ASTM B444, ASME SB444, AMS 5581
Tikanga | Te Kaha Toka | Te Kaha Tuku | Te whakaroa |
iti, ksi | iti, ksi | iti rawa, % | |
Kōeke 1 | 120 | 60 | 30 |
Kōeke 2 | 100 | 40 | 30 |
*Ka taea te whakarato i nga taonga kaha ake i roto i te ahua makariri.
incoloy 625 ngongo ngongo kapi
70°F | 200°F | 400°F | 600°F | 800°F | 1000°F | ||
---|---|---|---|---|---|---|---|
Kiato | lbs/in3 | 0.305 | - | - | - | - | - |
Te Roha Ngawha | X10-6/°F | - | 7.1 | 7.3 | 7.4 | 7.6 | 7.7 |
Kōwae Elastic | 103 ksi | 30.1 | 29.6 | 28.7 | 27.8 | 26.9 | 25.7 |
Poisson Ratio | - | 0.278 | 0.28 | 0.286 | 0.29 | 0.295 | - |
Te Whakawhitinga Ngawha | Btu-in/h·ft2·°F | 68 | 75 | 87 | 98 | 109 | 139 |
Te wera motuhake | Btu/lb·°F | 0.098 | 0.102 | 0.109 | 0.115 | 0.122 | 0.118 |
Te Kaha Tuku | ksi | 70 | 68 | 63 | 60 | 59 | 34 |
Te Kaha Toka | ksi | 140 | 134 | 130 | 129 | 129 | 88 |
incoloy 625 ngongo ngongo kapi
TE WHAKAMAHI TE WHAKAMAHI TE WHAKAMAHI TE KAUPAPA KAUPAPA KAUPAPA KAUPAPA KAUPAPA KAUPAPA KAUPAPA Oxygen Decarburization (VOD) Argon Oxygen Decarburization (AOD) ranei.Ka taea te whakarato i roto i te ahua o te reera, te wairewa, te ahua whakamaroke ranei.Ko te kaha o te kaha annealed ka whakamahia i roto i nga ratonga tae atu ki te 1100°F, i te wa e whakamahia ana te ahuatanga o te otinga ki nga tono kei runga ake i te 1100°F.